Technical parameters
Outside view: light yellow granular solids
Chemical types: fatty acid sodium
Apparent density: 0.69 kg/l
PH (5%) : approx. 10
This is a technical parameter, rather than the product range
Application:
Olinor 4020 used for deinking plant under the condition of alkaline ink in the operation of search agent.
Olinor used in 4020 can be directly added to the pulp but often dissolved the product first and before joining into the flotation especially mixing tank can achieve the best effect. If you want to get a good solution, the dissolution of 8-10% recommended preparation according to the following procedure:
Using 900-920 litres of hot water (greater than 60 ℃)
Under stirring and into the 80-100 kg Olinor 4020 and stir about 15 minutes
Preparation of the preservation of good solution temperature not less than 50 ℃
In order to use Olinor 4020 largest printing ink removal efficiency, water hardness requirements at least not less than 100 PPM calcium carbonate. Pulper in PH less than 8.5, and the best value between 10 and 11.
Particularly hard water (500 PPM calcium carbonate st13) will damage the flotation effect of raids.
Olinor4020 high purity and the consistency of the components will ensure that the most effect under the adding amount of low 4020, besides have the function of control bubble it's join white deinking pulp can also be achieved. The following recommendations formula, in newspapers and magazines as raw material of paper factory proved to be successful, but the audi, technical support staff will according to the specific requirement and situation of waste paper pulp factory to the quality of the concrete Suggestions are given.
1.0 3.0% sodium silicate (sodium silicate)
1.0 1.5% 100% sodium hydroxide
0.7-1.0% sodium peroxide 100% basis
0.1 0.3% complexing agent
0.2 0.6% Olinor 4020
According to the quality of the water, need to join an organic complexing agent, and sodium silicate was added to hydrogen peroxide stability. In our recommended products of organic chelating agent can prevent caused by using sodium silicate and silica scaling. This scale is connected because of sodium silicate and polyvalent metal ion.
The packing and shipping